Spunky Spray Sunscreen – CSW 003-67

Natural solubilizers and an oil soluble, non-irritant preservative make formulating this Spunky Spray Sunscreen a breeze. The film forming capability of Endicare® SC-520Q increases water-resistance properties and creates an even spray on the skin. With olive-based emulsifiers and shea butter, the skin is protected without a harsh or heavy feel.

Phase A
Deionized Water64.20%
Dissolvine® 220S1,2 (Tetrasodium EDTA)0.10%
Allantoin1,3 (Allantoin)0.20%
Endicare® SC-520Q1 (Polyethyloxazoline)5.00%
Phase B
Endipure™ SHEA1 (Butyrospermum Parkii (Shea) Butter)1.50%
Olivatis™ 111 (Polyglyceryl-3 Olivate Phosphate)1.00%
Viv-GMU1,4 (Glyceryl Undecylenate)1.00%
E-Vite1,4 (Tocopheryl Acetate)0.50%
Olivatis 13™1 (Polyglyceryl-3 Cetearyl Ether Olivate)4.00%
Endimulse® EGDS1 (Glycol Distearate)2.00%
Phase C
AllyEster™1,5 (Ethyl Palmate)4.00%
Endicare® TN1 (C12-15 Alkyl Benzoate)1.00%
Uvasorb MET1,3 (Benzophenone-3)3.50%
AVIS1,4 (Butyl Methoxydibenzoylmethane)1.50%
Cinnamon1,4 (Ethylhexyl Methoxycinnamate)7.50%
Octyne-B1,4 (Octocrylene)3.00%

Suppliers

  • 1Coast Southwest, Inc.
  • 2Akzo Nobel Functional Chemicals, LLC.
  • 33V
  • 4Vivimed Laboratories
  • 5Allyson Enterprises

Properties

  • pH: 5.85
  • Viscosity: spindle 3.0 at 100.0 rpm = 600.0 – 900.0 cst. Estimated SPF value available upon request. Aerosol compatibility available upon request.

Instructions

Phase A – Add Phase A in order to main vessel under shear mixing and begin heating to 80°C. Phase B – In a separate vessel, add Phase B materials under propeller or shear mixing and begin heating to 80°C. Phase C – In an additional separate vessel, add Phase C materials under propeller or shear mixing and being heating to 80°C. Note: This ensures proper solubilization of sunscreens before adding to actual oil phase. Once all materials in Phase C are uniform and clear, add Phase C to Phase B and continue mixing and heating. When Phase A and Phase B are at temperature, add Phase B to A slowly under very high shear mixing. Note: If emulsion is not “bright white” stronger mixing might be required, i.e. homogenization. Begin cool down. Once emulsion has cooled to 25°-30°C, transfer to final container.